P/N:
采用高纯度合成熔融石英制造
精密型合成石英核磁管采用高纯度合成熔融石英制造,Fe₂O₃含量低于0.005 ppm,在深紫外至近红外波段具有良好的透光性能。产品适用于光化学研究、变温核磁实验以及对材料纯度和光学性能有较高要求的NMR应用。
Wilmad 5mm O.D. Thin Walled Suprasil® NMR Tubes | |||||||
订货号 | 适用场强等级 | 长度 | 外径 | 同心度 | 弯曲度 | 内径 | 壁厚 |
535-PP-7SUP | 600 | 7" | 4.9635±0.0065mm | 13 µm | 6 µm | 4.2065±0.0065mm | 0.38mm |
535-PP-8SUP | 600 | 8" | 4.9635±0.0065mm | 13 µm | 6 µm | 4.2065±0.0065mm | 0.38mm |
535-PP-9SUP | 600 | 9" | 4.9635±0.0065mm | 13 µm | 6 µm | 4.2065±0.0065mm | 0.38mm |
528-PP-7SUP | 500 | 7" | 4.9635±0.0065mm | 25 µm | 13 µm | 4.2065±0.0065mm | 0.38mm |
528-PP-8SUP | 500 | 8" | 4.9635±0.0065mm | 25 µm | 13 µm | 4.2065±0.0065mm | 0.38mm |
528-PP-9SUP | 500 | 9" | 4.9635±0.0065mm | 25 µm | 13 µm | 4.2065±0.0065mm | 0.38mm |
507-PP-7SUP | 300 | 7" | 4.9635±0.0065mm | 51 µm | 25 µm | 4.2065±0.0065mm | 0.38mm |
507-PP-8SUP | 300 | 8" | 4.9635±0.0065mm | 51 µm | 25 µm | 4.2065±0.0065mm | 0.38mm |
507-PP-9SUP | 300 | 9" | 4.9635±0.0065mm | 51 µm | 25 µm | 4.2065±0.0065mm | 0.38mm |